[TheForge] Trenton Anvils

Andy Vida [email protected]
Tue Jan 22 12:20:31 2002


Not with Trenton's.  They welded some of their anvils at the waist.
The feet were of cast material and the face/horn/heel of wrought with
a steel plate welded on.

Ray Baker wrote:
> 
> Having it arc welded is not the norm. It shows an anvil whose original joint
> failed and had to be repaired.
> 
> Ray