[TheForge] Trenton Anvils

[email protected] [email protected]
Sun Jan 20 03:13:10 2002


i have a 100+/-  trenton... it is fairly clearly marked trenton on the side 
but right now dont remember there being a weight ... i am certainly not an 
anvil expert but it is my understanding they are a good anvil and i thing 
they are not cast