Andy Vida wrote:
>
> > Daniel Crowther wrote:
>
> > > I do not have any S-1, however I do have access to the following
> > > steels: A36, 5160, O-1, and automotive/truck engine valves. Which one of
> > > these would be my best choice?
>
> None of them will suffice.
I should have further qualified that with "if you want
convenience".
Their lack of hot hardness and general low grade of heat
tolerance will demand you work differently, taking care
not to draw the temper too much, rendering the tool useless.
Smiths used plain carbon steel for centuries and got the
work done. I did not mean to imply that the steels you
listed were of zero value. I meant to say that the high
alloy, heat tolerant steels allow you to work more conveniently.
My apologies for speaking neglectfully.