Ounce to guage is as follows:
36 oz - .048
32 oz - .0431
24 oz - .0323
20 oz - .0270
16 oz - .0216
12 oz - .0160
I believe there is also a 40 or 42 ounce
but I don't have the specs in front of me.
You may want to get a quote for an entire
sheet (3' x 8' is a common size) to save on
processing charges (assuming you need that
much).
- Matt
>From: "Miller, Ray (GEAE)" <[email protected]>
>Reply-To: [email protected]
>To: "'[email protected]'" <[email protected]>
>Subject: RE: [TheForge] Wholesale copper
>Date: Thu, 3 Jan 2002 06:45:41 -0500
>
>I think roofing copper is 16 oz. and they make flashing copper that I
>believe is 12 oz.
>and that is weight per square foot.
>
>Ray Miller
>Cincinnati
>
>
>
>-----Original Message-----
>From: lama [mailto:[email protected]]
>Sent: Thursday, January 03, 2002 3:09 AM
>To: [email protected]
>Subject: Re: [TheForge] Wholesale copper
>
>
>Kirsten, around here folks are paying $50 +/- per sheet for
>"roofing copper" I don't know the gague.
>dave m.
>
>----- Original Message -----
>From: K.A. S. <[email protected]>
>To: <[email protected]>
>Sent: Wednesday, January 02, 2002 1:43 PM
>Subject: Re: [TheForge] Wholesale copper
>
>
> > Copper and Brass Sales?
> > That's who I ordered from last time- reasonable prices, common carrier
> > delivery to the shop door. for 2 sheets of .054 thickness, 36"wx 96"l
> > copper plus the shipping, it cost about $511.
> > I lost the 800 number. The tele# on the bill is 847-490-9870
> > -Kirsten
> >
> >
> > >From: Buddy Holmes <[email protected]>
> > >Reply-To: [email protected]
> > >To: [email protected]
> > >Subject: [TheForge] Wholesale copper
> > >Date: Wed, 02 Jan 2002 08:07:06 -0600
> > >
> > >Folks;
> > >
> > >I was contacted by a copper wholesaler about two months ago. Good
>prices
> > >and would deliver to
> > >my door.
> > >I have since lost all the info. Misplaced his faxed price list, etc.
> > >
> > >They were located in either TX. AK or TN, just can't remember. Not
> > >Farmers Copper, not Atlas.
> > >
> > >Any help would be appreciated; supplies are low and need to get some
> > >better prices this new
> > >year for my next order.
> > >
> > >Many thanks;
> > >
> > >Buddy
> > >
> > >--
> > >Buddy Holmes
> > >Prairieville, LA
> > >
> > >Waterfall Forge
> > >http://www.waterfalling.com
> > >
> > >
> > >_______________________________________________
> > >http://mailman.qth.net/mailman/listinfo/theforge
> > >theforge mail list group photo site is
> > >http://albums.photopoint.com/j/AlbumList?u=1169182
> > >___________
> > >
> > >
> >
> >
> > _________________________________________________________________
> > Chat with friends online, try MSN Messenger: http://messenger.msn.com
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://albums.photopoint.com/j/AlbumList?u=1169182
> > ___________
> >
> >
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://albums.photopoint.com/j/AlbumList?u=1169182
>___________
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://albums.photopoint.com/j/AlbumList?u=1169182
>___________
>
>
_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp.