At 21:24 01/09/02, you wrote: >A good finish for outdoors is an outdoor rated lacquer with corrosion >inhibitors. Syncralac with Irgacore 153 for instance. > >Steve Smith And don't forget a high UV tolerance. I'd think that something with a top rated marine rating would be good in this respect. Dave