The porting from the cartridge to the cylinder chamber was 3/16 so
there was no way I could get the press to travel with that size port
(venturi), so I bored a hole in the end of the cylinder and welded in a pipe
coupling and solved one of the problems. The other line also went thru the
cast housing on the end, so I bored it out to 1/2" from 1/4 as that was
possible. The first one could not be done unless I cut the cylinder apart
and then did the machine work, and then rewelded it. So I had two days into
making a $20 cylinder work and I should have just gone and bought a new
cylinder and been done with it...........or waited until I found a regular
loader arm cylinder that would have fit the task.
Ralph
----- Original Message -----
From: "Ed Fasula" <[email protected]>
To: <[email protected]>
Sent: Saturday, January 05, 2002 11:39 PM
Subject: Re: [TheForge] 15Ton Press
> Hi Ralph,
>
> > This is a Sun control cartridge. You may have luck cutting the
bottom
> >off the cartridge, but mostly pilot controls of this sort also go along
with
> >small porting to allow minimal flow to outriggers or crane turn tables,
etc.
>
> Did you just try it and find it to be restricted or were you able to
figure
> out the porting was too small somehow?
>
> >Mine had to be
> >rebored for a new cylinder port and welded in..............that worked
for
> >me,
>
> The cylinder porting had to be re bored? What was welded?
>
> >getting all the oil out is a trick if the end that takes this cartridge
> >is loaded with oil in all the pores of the metal.
>
> I'm not following what you're talkin'bout!
>
> > It may not be ice......
> Looks like it was though. It stays out now.
>
> Ed
>
>
> _________________________________________________________
> Do You Yahoo!?
> Get your free @yahoo.com address at http://mail.yahoo.com
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge