[TheForge] 15Ton Press
Steve Smith
[email protected]
Sun Jan 6 00:12:01 2002
Consider putting the cylinder on the bottom and having a fixed top die/moving
bottom die. Steve Rollert has his press that way and it works fine.
I have a C style 35 ton press with the cylinder on top. It is over 7' tall and
weighs a ton (well, not that much). It would probably weigh a third as much if
it were both H frame and cylinder underneath.
Steve Smith
Ed Fasula wrote:
> Hi Chuck,
>
> >...have to be extremely tall to accommodate a 32" cylinder... There are
> enough advantages to my design over the cylinder on top that I
> >wouldn't recommend that route.
>
> Oops. Brain fart. 32" is the one for splitting wood. The press cylinder
> is 6"x24"
>
> Here is a link http://www.geocities.com/edfasula/smithing.html
> to a sketch of the current thought I have for a structure. I think I can
> keep it under 8' without too much worry. Please criticize now, not after I
> build it! What disadvantages do you see with the cylinder on top? While
> you're at it, let me know if you have any input on my plan with the pilot
> valve (there also). [Also not how I try to pass of images from my scanner
> as digital camera pictures.]
>
> >I'm not clear
> >on why you need to vary the motor speed in a hydraulic system.
>
> Because I'll probably split wood with the pump (run out the forge door with
> hoses with quick connects) and I want it to go fast enough. But I hear
> (here) that the pumps scream at 3600 rpm. I'm not sure what speed I want
> the ram to travel at. Some in the book went 2"/sec. That would take 3600
> rpm with the pump I'm looking at. So if I decided if I really wanted to
> run the press at that, I could, but sill turn it down for delicate work or
> if I was sick of the racket.
>
> >...why I'm using the C P
> >pump.The flow is full volume until you reach the maximum pressure.
>
> Do you know what ram speed full volume gives you?
>
> Hope you health is coming back well for you.
>
> Ed
>
> _________________________________________________________
> Do You Yahoo!?
> Get your free @yahoo.com address at http://mail.yahoo.com
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://albums.photopoint.com/j/AlbumList?u=1169182
> ___________