[TheForge] Wholesale copper

Peter Fels and Phoebe Palmer [email protected]
Thu Jan 3 22:34:01 2002


At 03:45 AM 1/3/02, you wrote:


Anyone notice how the price of retail copper  didn't follow the ton price 
back down?....Pete fels





>I think roofing copper is 16 oz. and they make flashing copper that I
>believe is 12 oz.
>and that is weight per square foot.
>
>Ray Miller
>Cincinnati
>
>
>
>-----Original Message-----
>From: lama [mailto:[email protected]]
>Sent: Thursday, January 03, 2002 3:09 AM
>To: [email protected]
>Subject: Re: [TheForge] Wholesale copper
>
>
>Kirsten, around here folks are paying $50 +/- per sheet for
>"roofing copper" I don't know the gague.
>dave m.
>
>----- Original Message -----
>From: K.A. S. <[email protected]>
>To: <[email protected]>
>Sent: Wednesday, January 02, 2002 1:43 PM
>Subject: Re: [TheForge] Wholesale copper
>
>
> > Copper and Brass Sales?
> > That's who I ordered from last time- reasonable prices, common carrier
> > delivery to the shop door.  for 2 sheets of .054 thickness, 36"wx 96"l
> > copper plus the shipping, it cost about $511.
> > I lost the 800 number.  The tele# on the bill is 847-490-9870
> > -Kirsten
> >
> >
> > >From: Buddy Holmes <[email protected]>
> > >Reply-To: [email protected]
> > >To: [email protected]
> > >Subject: [TheForge] Wholesale copper
> > >Date: Wed, 02 Jan 2002 08:07:06 -0600
> > >
> > >Folks;
> > >
> > >I was contacted by a copper wholesaler about two months ago. Good prices
> > >and would deliver to
> > >my door.
> > >I have since lost all the info. Misplaced his faxed price list, etc.
> > >
> > >They were located in either TX. AK or TN, just can't remember. Not
> > >Farmers Copper, not Atlas.
> > >
> > >Any help would be appreciated; supplies are low and need to get some
> > >better prices this new
> > >year for my next order.
> > >
> > >Many thanks;
> > >
> > >Buddy
> > >
> > >--
> > >Buddy Holmes
> > >Prairieville, LA
> > >
> > >Waterfall Forge
> > >http://www.waterfalling.com
> > >
> > >
> > >_______________________________________________
> > >http://mailman.qth.net/mailman/listinfo/theforge
> > >theforge mail list group photo site is
> > >http://albums.photopoint.com/j/AlbumList?u=1169182
> > >___________
> > >
> > >
> >
> >
> > _________________________________________________________________
> > Chat with friends online, try MSN Messenger: http://messenger.msn.com
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://albums.photopoint.com/j/AlbumList?u=1169182
> > ___________
> >
> >
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://albums.photopoint.com/j/AlbumList?u=1169182
>___________
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://albums.photopoint.com/j/AlbumList?u=1169182
>___________