[TheForge] Rivets and Bronze
Steve Smith
[email protected]
Tue Jan 1 23:22:01 2002
Silicon bronze forges pretty well. You have to be careful about heat. It seems to me that you don't want any hotter than a very dull red glow, and if
it gets too cold it can break. You tell too cold by feedback from your hammer.
Steve Smith
"Hufford, David" wrote:
> Anyone know a source of button head copper rivets? Bee Industries only has brass. Anyone know about Cobb & Drew; do they have non-ferrous rivets?
>
> Also, what is the best bronze alloy for forging? Is silicon bronze OK? How about phosphor bronze?
>
> Thanks for any enlightenment anyone can provide.
>
> David Hufford
> Richmond KY