David;...the harder the material, the steeper the edge.


>usual angle for a cold chisel is 60 degrees.
>
>"Hufford, David" wrote:
> >
> > What is the usual angle of the blade (cutting edge) of a cold 
> chisel?  Is there a standard, or does this vary?
> >
> > David Hufford
> > Richmond KY USA
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://albums.photopoint.com/j/AlbumList?u=1169182
> > ___________
>
>--
>         -Andy V.
>         Eventide Forge
>         Mad Science Inc.
>         Scottsdale, AZ
>
>         A sense of Good Enough is one of the tools you need in your shop.
>         I'll tell you, the gods will spot you 90%.  Then, if you like, 
> you may
>work
>         it up a little, you'll maybe get 96%, if you're real good, 98%.  Be
>         satisfied.  That last 2% is Heaven's prerogative.  If it's granted,
>offer
>         prayers and praises, but on no account try to force your way up 
> there.
>         Points will ALWAYS be deducted for Hubris.
>                                                         RtH
>
>         I hold the keys to the sea of possibilities.
>
>                                                         -Patti Smith
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://albums.photopoint.com/j/AlbumList?u=1169182
>___________