In the book "Metal Fabricator's Handbook" by Ron & Sue Fournier they speak
of gas welding Al using flux by Alcoa but also mentions several others. He
points out that it is for "non-structural" parts. I tried it several years
back with limited success, but admit I don't weld well, and did not try
real hard.
Larry
Cameron Stoker wrote:
> On Wed, Feb 06, 2002 at 05:40:39PM -0500, Dan Tull wrote:
> > What flux do you use for aluminum forge welding in a gas forge?
>
> This may or may not be related, but I have been hunting around for
> aluminium Oxy-Fuel welding flux. This is the closest I have come (and a
> pretty good source of information, too):
>
> http://tinmantech.com
>
> at the very bottom of this page there is info on welding flux:
> http://tinmantech.com/html/aluminum_gas_welding__brazing_.html
>
> I read alot of this site and was feeling inspired. I tried welding up
> some 6061 with 5356 rod using some leftover anhydrous borax. I think it
> would work great - I forgot that I had put wd-40 in my spraycan instead
> of the alcohol I normaly keep it full of. So my de-greasing of the
> surfaces was really a greasing. Didn't get very good penetration.
>
> But I have to say that I really like the idea of gas welding the 6061.
> TIG is what I have been using on it, but it takes a long time to heat
> up some bigger chunks, and the penetration is really hard to get just
> right.
>
> I had never tried gas welding Al ever since I tried to cut it once with
> the cutting torch and just made a big puddle. I thought its transition
> zone was too narrow to be reasonable to work with.
>
> Anybody on the list have experiences gas welding Al?
>
> Anybody know how long it takes 6061 to age harden at room temp from an
> anneal/solutionizing heat?
>
> --
> Cameron Stoker
> "May you run like a vicuna!"
> [email protected]
> www.stoker.net/cameron/pgp <- public key
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________