> On Wed, 13 Feb 2002 10:59:52 +1030, Shannell wrote:
>
> >While on the sand casting topic (barely :)) saw a good tip the other day,
> >use fine grade cement mix and 10w motor oil as your casting mould
material,
> >very fine detail and easily available.
>
> Don't use "cement", what you want is "finishing mortar".
> It's all fines, no grit or lumps.
>
>
>