Deep pots are, for the long term, overcome with a more powerful fan rather
than putting the iron down in the pot. For the relatively small items I
make, I like a 4 1/2" deep pot. Great for burning the oxygen out of the
fire and for forge welding. I like the Centaur high powered blower and
wouldn't use anything less, unless I didn't have one. I also like the depth
and size of the standard Centaur fire pot. They are about 4 1/2 " deep if
you plug up the end depressions which I do. The big problem with the
Centaur fire pot is that they are thin, approx. 3/8" and burn out much
quicker than some of the 3/4" thick ones. The last firepot I made to the
size of the Centaur and made it out of mild steel 5/8" for the big flat
sides and 3/8" for the bottom and ends. Again, here is my 2 cents worth.
Dick
----- Original Message -----
From: "wmullett" <[email protected]>
To: <[email protected]>
Sent: Thursday, February 07, 2002 6:50 PM
Subject: RE: [TheForge] Fire pot depth - opinions wanted
> Actually, I think too deep is a problem. If the pot is deep you end up
with
> your stock at an angle and one end is always in a bad area. If the sides
> aren't cut down already, you'll end up doing it.
>
> On the other hand, if the pot is shallow and as Bruce says, you can always
> make it deeper by adding brick around the sides or just mounding up your
> coal.
>
> Walt
>
> > -----Original Message-----
> > From: [email protected]
> > [mailto:[email protected]]On Behalf Of Bruce Freeman
> > Sent: Thursday, February 07, 2002 8:56 AM
> > To: [email protected]
> > Subject: Re: [TheForge] Fire pot depth - opinions wanted
> >
> >
> > I've successfully worked small stock (not over 3/4" thick)
> > over pots ranging from 2" to 6" deep. It's not the depth of
> > the pot but the depth of the coal. A flat table with a
> > tuyere pipe would do fine if you piled the coal up high
> > enough for the work at hand. Put a few firebricks around the
> > coal to keep it from spreading across the table and you don't
> > need a pot at all.
> > Bruce Freeman
> >
> > >>> Frederick Faller <[email protected]> 02/06/02 05:43PM >>>
> > OK folks, what is the best depth for a forge firepot.
> >
> > Please support your opinions with reasons :-)
> >
> > Frederick Faller
> >
> > __________________________________________________
> > Do You Yahoo!?
> > Send FREE Valentine eCards with Yahoo! Greetings!
> > http://greetings.yahoo.com
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>