I've often wondered about this as well.
> With all the recuperative appliances the idea is that the hotter the
> combustion air, the hotter and more efficient the fuel conversion is.
Or does it actually work against the combustion process because
hot air is less dense. Dodge experimented with Intercooled aspirated car
engines on the principal that colder air is denser and will give more
oxygen for the same volume. The HP did increase, so it worked for them.
Is there something else going on that makes preheating for forge
combustion good and bad for auto combustion?