[TheForge] tumbling media
[email protected]
[email protected]
Sun Feb 3 23:47:00 2002
Hi
Find out where they get the black stuff that they use in the ash trays at movie theater and other places, I have about 300lbs that was tossed out . I mixed that in with small chunks of ceramic from a toilet tank I broke up, works great.
Bob Hendricks
Gulfport Ms.
------------------------------------------------------------
>
> From: "Jack Parks" <[email protected]>
> Date: 2002/02/03 Sun PM 08:38:04 EST
> To: "the forge" <[email protected]>
> Subject: [TheForge] tumbling media
>
> What is a good locally available, cheap madia for removing rust and paint
> from old cast iron parts? I am currently using sand blast sand and some
> limestone gravel thrown in for a more aggressive mix. It still isn't as
> aggressive as I would like it to be. How would 1/4"-1/2" crushed quartz
> work??? This can stand to save me countless hours standing at the sand blast
> cabinet. thanksJack Parks , [email protected] ,Fire Steel Forge
> Dakota Artist Blacksmiths Assoc.
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>