What is a good locally available, cheap madia for removing rust and paint
from old cast iron parts? I am currently using sand blast sand and some
limestone gravel thrown in for a more aggressive mix. It still isn't as
aggressive as I would like it to be. How would 1/4"-1/2" crushed quartz
work??? This can stand to save me countless hours standing at the sand blast
cabinet. thanksJack Parks , [email protected] ,Fire Steel Forge
Dakota Artist Blacksmiths Assoc.