On Sat, 02 Feb 2002 12:05:11 -0600, Dave Brown wrote:

>stick.  You can "push" the puddle around and with practice (more than I 
>have to date)

	Go down one orifice size and up your pressures about 5%. 
The smaller the flame with a higher pressure behind it, the better
the puddle can be moved.  With practice (the best instructor), you
can make torch welds that are completely invisible - it looks like
a one-piece casting.