[TheForge] shrink fit techniques

Williams, Mark E. [email protected]
Fri Feb 1 12:58:12 2002


All:

A safer bath is dry ice and methanol (wood alcohol). Make sure the dry
ice is in small pieces so it forms a slurry with the liquid.=20

Mark

Mark E. Williams, PhD
Department of Mathematics and Computer Science
University of Maryland Eastern Shore
Princess Anne, Maryland 21853
410-651-6431 or 6420
=20

-----Original Message-----
From: Roy Wilson [mailto:[email protected]]=20
Sent: Friday, February 01, 2002 11:54 AM
To: [email protected]
Subject: Re: [TheForge] shrink fit techniques

On Fri, 1 Feb 2002 11:46:22 -0500, RW wrote:

>Ray, is dry ice in a zylene bath something readily doable in a small
one-man
>shop?  What precautions should one take?    RW

	Tongs, face shield, heavy gloves.  Acetone in dry ice works
well too, and is usually cheaper than xylene.



Roy Wilson
General Operations Director
Zanzibar Internet Land Line Administrator



_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  [email protected]
password:  anvil