[TheForge] Bradley Hammers, Hammer madness

thermoss [email protected]
Sat Dec 28 09:42:00 2002


where did you order a bushing for the beaudry from?

----- Original Message -----
From: Ralph Sproul <[email protected]>
To: <[email protected]>
Sent: Friday, December 27, 2002 3:35 PM
Subject: Re: [TheForge] Bradley Hammers, Hammer madness


>         Steve, The work marathon continues, so the Beaudry got
> dissassembled, bronze bushing pulled, new busing ordered..........and
there
> she sits.   Maybe this spring things will allow a couple days to put it
> together and make her spin.
>
> Ralph
>
>
> ----- Original Message -----
> From: "Howell Steve" <[email protected]>
> To: <[email protected]>
> Sent: Wednesday, December 25, 2002 6:09 PM
> Subject: RE: [TheForge] Bradley Hammers, Hammer madness
>
>
> > Will do, Ralph. I pretty much characterized every aspect of the rebuild
so
> if pictures of bearing journals & ram guides interest you, then I can
> scratch that itch~  Real WORK pictures are soon in coming.
> > BTW- how's the Beaudry coming?
> >
> >
> > Steve Howell
> > Seattle
> >
> >
> > -----Original Message-----
> > From: Ralph Sproul [mailto:[email protected]]
> > Sent: Wednesday, December 25, 2002 7:31 AM
> > To: [email protected]
> > Subject: Re: [TheForge] Bradley Hammers, Hammer madness
> >
> >
> >         Steve, Great to hear you've got your hammer up and running, post
> or
> > send along a picture would you?
> >
> > Ralph
> >
> >
> >
> >
> > --- StripMime Report -- processed MIME parts ---
> > multipart/alternative
> >   text/plain (text body -- kept)
> >   text/html
> > The reason this message is shown is because the post was in HTML
> > or had an attachment. Attachments are not allowed.
> > Please post in Plain-Text only.---
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login:  [email protected]
> > password:  anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>