[TheForge] New hammer
Dave Brown
[email protected]
Sat Dec 14 22:35:00 2002
At 22:09 12/14/02 -0500, you wrote:
>Smashed up a piece of wood with my new Kinyon style hammer tonight.
>I'm just waiting now for the dies to heat up for welding. Heat treat
>them tomorrow and make up a control treadle and its done at last. I
>will put up pictures in a day or two.
>
>John
Looking forward to seeing the pictures. I note that you said "Kinyon style
hammer". Does that mean you deviated somewhat from Ron Kinyon's plans, or
did you follow them according to the original plans? I'm curious because I
have most of the parts for making one myself. Just need the pneumatic
cylinder and the plumbing stiff, bit I've got the heavy stuff ready to go.
Dave Brown
Heritage Smithing
Green Bay, WI
ABANA, UMBA, GoM, MODA, ARG