[TheForge] New Style Lil Giant Dies

Ed F [email protected]
Sat Dec 7 20:05:01 2002


What's MG750 welding rod?

----- Original Message -----
From: "Dan Tull" <[email protected]>
To: <[email protected]>
Sent: Saturday, December 07, 2002 6:02 PM
Subject: Re: [TheForge] New Style Lil Giant Dies


> I've used MG750 rod on mild steel plates for years
>
> dan tull
> georgia
> abba, afc, S.C. psba, obg,sofa
> ----- Original Message -----
> From: "Ed F" <[email protected]>
> To: <[email protected]>
> Sent: Sunday, December 01, 2002 1:01 PM
> Subject: Re: [TheForge] New Style Lil Giant Dies
>
>
> > I was thinking of making some texturing dies out of mild steel plate and
> > using hardfacing rod (or maybe I can find something I can use the TIG
> welder
> > with) for texture.  Has anyone played with that?
> >
> > Ed
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login:  [email protected]
> > password:  anvil
> > ___________
> >
> >
> >
> >
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>