Turns out it is silicone modified UHMW. Coefficient of friction is .15-.20
static and .9-.12 dynamic. Hardness, Durometer Shore D 67-70
I have the full sheet of physical properties scanned if anyone wants it
email me at [email protected]
It is made in 3/8" and 1/2" sheets
You can get it from Precision Punch, 800-233-4516. Ask for Barbara.
Ed
----- Original Message -----
From: "Larry Brown" <[email protected]>
To: <[email protected]>
Sent: Saturday, November 30, 2002 7:43 AM
Subject: Re: [TheForge] Making power hammers
> Any more info?
> L Brown
>
> At 10:15 PM 11/29/2002 -0600, you wrote:
> >A company just send me a sample of oil impregnated UHMW. Sounds like it
> >could be the thing
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>