Steve, In addition to what Dave just wrote about this being a
"charged" system....... that alone tells you you are working against air
cushions in the opposing chambers of the cylinder. This leds to great
control and a yo-yo like bounce that the shuttle valve yields when the
exhaust is "feathered". It is a hard hitting hammer when open wide as the
air pressure and ram weight are working for you. The return is aided by the
bounce off the anvil or work, and I find I use the air hammer more than my
50 lb little giant.
A 5 hp compressor keeps up with my hammer.
The points of the self contained hammers is the positive
displacement the rear air system supplies.......so if you are half way thru
a stroke - you let off the treadle and the ram is then powered up so you can
literally pull a ram out of the stroke with the self contained hammers.
The trick to the valves to me seems to be dealing with "all the air"
it just dosn't go all to running the hammer or all to returning the
ram........it is the balancing of the "spill" that isn't required to do
either funciton when you are feathering the treadle for light hits verses
all out force of the machine.
Ralph
----- Original Message -----
From: "Steve Smith" <[email protected]>
To: <[email protected]>
Sent: Sunday, December 01, 2002 7:15 PM
Subject: Re: [TheForge] Krause/Nazel type air hammer
> Well, I'd like something larger than my current 25 pound LG. This gets
> into a 5-7.5HP compressor pretty quickly from what I hear.
>
> I don't mean to bad mouth the Kinyon design; from what I understand (I'm
> hoping Dave M. will jump in and improve me), Kinyon's push on one side
> of the piston, then push on the other side. You can do a lot of work on
> this style hammer, but it doesn't seem like you have a lot of control of
> the ram position.
>
> Steve
>
>
>
> [email protected] wrote:
> > steve,
> >
> > the idea is pretty straightforward but the transfer of idea to reality
has not been so straightforward as one would hope. krause demoed his hammer
over two years ago. if it was a workable idea and so much better than the
kinyon you would think they (krausehammers) would be all over by now.
> >
> > there has been a lot of talk over on the keenjunk site about this
project. mark krause was posting about his effort to upscale his design to a
larger size. also a guy named john larson has had some success. there is a
search feature at the keenjunk site to search for their postings.
> >
> > i'm surprised that none of the kinyon builders haven't responded to your
comment about kinyons "just bounces between top and bottom". from what i
hear the kinyon hammers are doing a fair amount of work as they bounce. also
a "very large compressor" isn't needed unless you do very large work. check
out larry zoellers downsized kinyon that runs off a fairly small affordable
compressor.
> >
> > bob (still using a 25lb LG)
> > _______
> >
> >
> >>The idea is pretty straightforward. You use a motor to drive a double
> >>acting air cylinder. This is connected to the ram air cylinder (also
> >>double acting) via the air ports. The air provides the give in the
> >>hammer that is done in a Little Giant with a spring and toggle arms.
> >>
> >>The big advantage over the Kinyon style is control. The Kinyon hammer
> >>ram just bounces between top and bottom (or the top and the work). The
> >>Kinyon can only push the ram from one side at a time (assuming I
> >>understand how the Kinyon works...). The Krause/Nazel hammer applies air
> >>to both sides of the piston. The side with the most pressure dictates
> >>which way the ram will move. The pressure can be reversed immediately by
> >>changing the foot treadle position (and altering the balance of
> >>pressure). This makes it much more responsive.
> >>
> >>It is also a way to avoid buying a very large compressor that I don't
> >>have a lot of other use for. Since I'm doing this for fun, I get to
> >>build it myself and mess around with something different.
> >>
> >>Steve
> >>
> >>mike wolfe wrote:
> >>
> >>>
> >>>Steve Smith wrote:
> >>>
> >>>
> >>>>I'm starting on building a Krause/Nazel type air hammer,
> >>>
> >>>
> >>>
> >>>Steve:
> >>>Tell me more about the Krause/Nazel type air hammer, I had seen it in
> >>>operation at the conference, and I had been waiting for Mark to go
> >>>further with its evolution, I also thought "Sid" was getting involved
> >>>with the project a while back.
> >>>I have not heard anything for a while until you had talked of it.
> >>>Are there new plans or new developments about the Krause/Nazel type air
> >>>hammer.
> >>>Any info would be wonderful..
> >>>
> >>>Thanks
> >>>Mike Wolfe
> >>>
> >>>
> >>>
> >>>_______________________________________________
> >>>http://mailman.qth.net/mailman/listinfo/theforge
> >>>theforge mail list group photo site is
> >>>http://www.photoaccess.com
> >>>Login: [email protected]
> >>>password: anvil
> >>>___________
> >>>
> >>>
> >>>
> >>
> >>_______________________________________________
> >>http://mailman.qth.net/mailman/listinfo/theforge
> >>theforge mail list group photo site is
> >>http://www.photoaccess.com
> >>Login: [email protected]
> >>password: anvil
> >>___________
> >
> >
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>