Andy,

Try thinning it some.  The thinner is also lighter than water and should 
help with the flotation.

Dave

At 19:30 12/01/02 -0800, you wrote:
> > What kind of paint are you using?
>
>Ace gloss oil enamel (any color as long as it's black)