[TheForge] New Style Lil Giant Dies
Ralph Sproul
[email protected]
Sun Dec 1 16:38:01 2002
Make some 1 1/4" buttons with five or six welds across the
top.......the pounds per square inch increase dramaticly when you go from a
full die to a small round with texture. The results are instant and much
easier on the dies. This is the perfect example of what to do with those
dies going to the lower bolt on section you were refering to earlier.
Ralph
----- Original Message -----
From: "Ed F" <[email protected]>
To: <[email protected]>
Sent: Sunday, December 01, 2002 1:01 PM
Subject: Re: [TheForge] New Style Lil Giant Dies
> I was thinking of making some texturing dies out of mild steel plate and
> using hardfacing rod (or maybe I can find something I can use the TIG
welder
> with) for texture. Has anyone played with that?
>
> Ed
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>