Bruce,

Pure Iron and wrought are cool to work with, but I seem to do pretty well
with A36.
I would certainly being willing to stock some PI maybe a hundred lbs.  For
most of my work I prefer the strength of the steel. That being said, getting
something that forge welds easier and faster than A36 would be nice.  $73K
is a pretty big number to have invested in stock.

David
----- Original Message -----
From: "Bruce Freeman" <[email protected]>
To: <[email protected]>
Sent: Tuesday, August 27, 2002 10:05 AM
Subject: Re: [TheForge] Pure iron - a possible solution.


> No, there are no extra zeros here:
>
> ~$73,000 for ~70,000 lbs, including shipping.
>
> Is that clear?
>
> Bruce Freeman
> NJ
>
>
>
> >>> <[email protected]> 08/27/02 09:56AM >>>
> Are there extra zeros here?
>
> >
> > I have corresponded privately with Michael about PI.  It seems the
entire
> > inventory could be bought for ~$73000 for 70000 pounds of PI, including
> > shipping (2 truck loads), storage racks and a power hack saw.
>
>
>
> ___________
>
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>