[TheForge] it almost works:-)
jacques gallant
[email protected]
Wed Aug 28 12:23:03 2002
I had another try at getting my propane forge up to heat, and learned the
importance of waiting for it to warm up for five or ten minutes. I also
stacked fire bricks at BOTH ends this time, and managed to get the inside of
the forge(a light coating of fireclay on top of ceramic fibre insulation) to
glow orange all over. This was acheived useing anywhere between 10 and 20
psi of propane and just the right amount of air... so it almost works.
Still it was painfully slow watching a 5/16" rod getting up to forgeing
heat, barely hot enough for upsetting.
Dave M recommended a High Pressure regulator, so I called the welding supply
company and they have one with NO PRESSURE GAUGES that will deliver between
10 and 250 psi. It's the sort of thing people around here use for burning
blueberries and big lobster boils... Is this what you guys use on your
forges?
_________________________________________________________________
MSN Photos is the easiest way to share and print your photos:
http://photos.msn.com/support/worldwide.aspx