[TheForge] Sheet metal roller qestion

Walter L. Mullett [email protected]
Sun Aug 18 14:27:00 2002


Actually Ray, I have two adjustments on this unit.  One is the "thickness"
between the two rollers and the other is the outside roller for diameter of
the finished roll.

Is the small diameter round stock rolled sheet metal or is it steel rods for
hems?

-----Original Message-----
From: Ray Miller <[email protected]>
To: [email protected] <[email protected]>
Date: Sunday, August 18, 2002 12:31 AM
Subject: Re: [TheForge] Sheet metal roller qestion


>The grooves on the end of the roll are to roll small diameter round
>stock. Usually something like 3/8" and smaller. Each groove for a
>different diameter. As fas as diameter rolling sheet stock, you adjust
>that with the screw adjustment. (It isn't really a thickness
>adjustment). You start out fairly loose and roll your stock through.
>Keep tightening up on the adjustment until you get the diameter you
>want. (Tighter adjustment smaller diameter roll).
>
>(I;m not Dave Brown but I thought I might cast in my two cents).
>
>And $7 is a steal!!
>Ray
>Cincinnati
>
>Walter L. Mullett wrote:
>
>>Dave brown can probably answer these:
>>
>>I picked up a clean, antique sheet metal roller today.  It's got 3 - 30"
>>rollers with two geared together and one of those has a crank.  Small
>>adjustment on the top roller for metal thickness.  Each roller is about
>>1-1/2" and the outfeed roller is screw adjustable from an almost parallel
>>position with the bottom roller to almost parallel with the upper roller.
>>The name on it is "ULSTER".
>>
>>The outfeed and bottom roller both have about 4 grooves near one end with
>>each being a little different in size.  I assume that would be for a hem
>>turned out?
>>
>>What kind of diameter could I get with this?
>>
>>I think I stole it at $7 but my better deal was a Lincoln 225 AC welder
with
>>50# of rod, 2 helmets and a cart for $30.   HUGE SMILE
>>
>>Walt
>>
>>
>>
>>
>>
>>
>>_______________________________________________
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login:  [email protected]
>>password:  anvil
>>___________
>>
>>
>>
>
>
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  [email protected]
>password:  anvil
>___________
>
>