I was at and auction today in the W. VA. pan handle that had what they called a cannon ball anvil. It was hornless, about 200 lbs with hardie hole at each end. On the sides of the anvil were various ladle type depressions. It was obvoiously cast and came out of a shop nearby. Has anybody seen an anvil like this? This one went for around $800. Walt