Oh boy, here we go again. Put the horn where ever you want it but try to
roll a ring around the horn pointed right if you are right handed.
Ralph Macey
Wood 'n Iron
Warrenton, MO
>
> Point the horn to the left, forget and leave a hardy in the hole, hit the
> hardy with your right hand as you start to hammer and then you will have
the
> horn pointed in the correct direction when you have to start hammering
with
> your left hand.
>
> It only took me once (a small skin) to remember that one of the first
> things that Dan Tull taught me was "horn to the hammer hand side". I was
> not the first to have this happen and will not be the last. It only took
me
> one time to learn, I learn fast.
>