[TheForge] cast iron - Little Giant pulley
Dave Brown
[email protected]
Fri Aug 9 16:52:01 2002
The casenite will only give you a superficial hardening suitable for wear
resistance only. It won't do a thing for hardening against the impact
received by your hammer dies.
Dave Brown
>On Fri, 9 Aug 2002 11:16:18 -0600 Cameron Stoker <[email protected]>
>writes:
> > Also, I've been thinking of making some new hammer dies from a36 and
> > then
> > casehardening them with casenite. Has anyone tried this? I worry
> > that the
> > case won't do much to stop the die from deforming deeper down in the
> > body
> > of the die. I can't really afford $250-$350 per set of dies, and it
> > is a
> > real pain to machine tool steel on my 3-in-1 mill.
> >
>
>
>________________________________________________________________
>GET INTERNET ACCESS FROM JUNO!
>Juno offers FREE or PREMIUM Internet access for less!
>Join Juno today! For your FREE software, visit:
>http://dl.www.juno.com/get/web/.
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: [email protected]
>password: anvil
>___________