[TheForge] RE: burner flares
Mike Sweany
[email protected]
Thu Apr 25 11:10:01 2002
I dunno i forged mine. until they looked about right.
If plumbing fittings work machining shouldn't be necessary.
The simple formulae I use is more air= bigger flare. less air=smaller flare
---------------------------------
Do You Yahoo!?
Yahoo! Games - play chess, backgammon, pool and more