[TheForge] filling pits
John Chobrda
[email protected]
Sun Apr 21 10:08:00 2002
I would check with your powder coater to see what he uses. There are some metal
filled epoxies on the market (muffler patch etc.) but I don't know if they are
compatible with the powder coating process. The bigger problem is with your
welding set up, you should not be getting pits in your welds, sounds like
porosity.
John C.
irontree wrote:
> Hi all,
> Anyone know a good way to fill pitting leftover from arc welding
> (without grinding them). I ground everything smooth but a few pits are too
> deep. I could fill them but there are lots of little ones. The lamps I am
> making are going to be powder coated so color of the patch doesn't matter
> but the patching should be bake proof.
>
> Plaster? plumbers putty, epoxy filler?
>
> Thanks
>
> Dan
> www.visi.com/~irontree
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil