Today my roommate, the squid, came home with some power hacksaw blades.
They're 22" long, 1 1/2 " wide, and about 1/16 "+  thick. They say,
"Brazil Starrett high- speed steel REDSTRIPE Hacksaw- re-order RS
2104-8. What kind of steel have I got, and what will I need to do to
soften it to re-forge and shape, then re-temper? I see new cooking
knives and a short-sword in my future.....