One can friction cut stainless on a bandsaw with the blade turned backward
or just dull, works good on thin stock, I have cut 3/8. Rowland
----- Original Message -----
From: "Larry" <[email protected]>
To: <[email protected]>
Sent: Friday, April 05, 2002 5:57 AM
Subject: Re: [TheForge] Cutting Stainless
> I agree with Steve, been using mine for years, I just get good blades from
> Granger or such and go to town on mild and carbon steel, brass and 304/316
> stainless. I use a blade with as many teeth I can find on the stainless.
>
> Larry
>
> Steve Bloom wrote:
>
> > At 12:01 AM 4/5/2002 -0500, Bill Wooley wrote:
> > >Can anyone suggest a decent band saw that will make nice precise cuts
> > >without putting me in the poorhouse? Are these Chinese and Taiwanese
> > >saws that Enco etc. sell worth looking into? I would much rather buy
> > >American or German. Better yet, does anyone know where there is a good
> > >used one driving distance from Phila. area? Any and all help greatly
> > >appreciated.
> >
> > I've been using the Harbor Freight ~$170 saw (sometimes as cheap as
> > $150 on sale) for 10 years or so. With a good bimetal blade, it does a
> > reasonable job -- a cut on a 3" x 6" piece of mild steel may be off be
> > < 1/8" over the 3" dimension. Since you can adjust the angle of the
> > blade on the horizontal dimension, you just have to set up a good 90
> > degree cut (and then mark the table). It isn't high precision, but it's
> > adequate. After 10 years of use, my saw is getting cranky - but for
> > $17/a year, I can't complain.
> >
> > Steve
> >
> > Steve Bloom, IronFlower Forge. Archer, FL
> > Webmaster for the FABA web site:
> > www.blacksmithing.org
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>