On Mon, 31 Dec 2001 09:32:21 -0500, Hufford, David wrote: >What is the usual angle of the blade (cutting edge) of a cold chisel? Is there a standard, or does this vary? It varies by make and model, but it's generally a bit shy of 30d from centerline (each side). Roy Wilson General Operations Director Wilson Eclectics