[TheForge] propane forge forced air
Adam Whiteson
[email protected]
Fri Dec 21 11:01:30 2001
Sounds like you are running too lean - too much air will cause excess
scale (free oxygen) and will also rob the forge of heat. I would try
increasing the jet size in *small* steps.
Adam
At 11:49 AM 12/20/2001 -0800, you wrote:
>I have a nc tool 2 burner knifemakers forge. recently I decided to build a
>manifold and add a forced air blower.
>The manifold blows air through the venturi openings. I put a air gate on the
>"in " side of the blower to control the air flow .
>I am not seeing a great difference in the efficiency of the forge and the
>scale seems worse than without the forced air. do I need to adjust the size
>of the jets? larger or smaller?also the back of the forge is not getting as
>hot as the front. any suggestions?
>
>----- Original Message -----
>From: Mike Linn <[email protected]>
>To: <[email protected]>
>Sent: Wednesday, December 19, 2001 10:01 PM
>Subject: Re: [TheForge] Re: hot vs cold rolled
>
>
> > I got about 120 feet of A36 1/4" round 2 years ago , and I'll bet my last
> > Dollar it was close to 1095. It was so brittle it shattered like glass
> > after a water quench. We use a lot of that size for s-hooks, match holders
> > and plant hooks at demos. You forge one end the cool it off to forge the
> > other. Damn stuff would break every time.....
> >
> > mike
> >
> > At 07:06 AM 12/20/01 -0800, you wrote:
> > >Yes, cold rolled has more strict requirements than hot rolled. Hot
> > >rolled is no longer 'mild steel' it is A-36. The tolerances are large.
> > >You may find a bar of A-36 that will analyze out close to cold rolled but
> > >the next will damn near qualify as tool steel. At one time I had the
> > >chemical analysis for both cold and hot rolled but have no idea where it
> > >is now. Maybe someone on the list will post it, I would like to see it
> > >again.
> > >
> >
> > Michael Linn
> > Artist Blacksmith
> > McCalla, Alabama
> > AFC Webmaster
> > http://afc.abana-chapter.com
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://albums.photopoint.com/j/AlbumList?u=1169182
> > ___________
> >
> >
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://albums.photopoint.com/j/AlbumList?u=1169182
>___________