>Anybody have a source for buying online, S1 steel.  I tried carpenter
>direct, they only have S7.
>
>Thanks
>
>John Elliott
>_______________________________________________


john,

sid suedmeier (little giant) had an ad in the last anvils ring (p.50) selling "crucible s-1 atha pneu" 5/8"-3/4"-1" in 2' lengths. phone is 402 873 6603

bob s.