[R-390] Ping Tests and Solder
Curt
cptcurt at flash.net
Mon Feb 27 15:07:29 EST 2012
It just SMELLS right!
On 2/27/2012 2:55 PM, rbethman wrote:
> I still use Kester #44.
>
> I've got a couple 1lb rolls. I'll keep using and buying until II have
> NO choice!
>
> Bob - N0DGN
>
> On 2/27/2012 2:32 PM, chacuff wrote:
>> I don't like the "unleaded" solder. Until I can no longer buy the leaded
>> type I will use it. The unleaded type doesn't seem to flow out as nicely as
>> the leaded.
>>
>> Just a personal thing I guess.
>>
>> I do like the Silver bearing solder it works really well and seems to be
>> harder. I use it in situations where physical characteristics benefit a
>> stronger solder connection.
>>
>> Cecil
>>
> ______________________________________________________________
> R-390 mailing list
> Home: http://mailman.qth.net/mailman/listinfo/r-390
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:R-390 at mailman.qth.net
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
More information about the R-390
mailing list