I don't like the "unleaded" solder.  Until I can no longer buy the leaded 
type I will use it.  The unleaded type doesn't seem to flow out as nicely as 
the leaded.

Just a personal thing I guess.

I do like the Silver bearing solder it works really well and seems to be 
harder.  I use it in situations where physical characteristics benefit a 
stronger solder connection.

Cecil
----- Original Message ----- 
From: "Barry" <n4buq at knology.net>
To: <r-390 at mailman.qth.net>
Sent: Monday, February 27, 2012 1:16 PM
Subject: Re: [R-390] Ping Tests and Solder


>> Yeah, I know "it's just solder" and pretty much any good non-acid-core 
>> will
>> do but thought I'd spark some new conversations.
>> Thanks guys,
>> Barry - N4BUQ
>
> Also, any comments on lead-free solder?
>
> (...and I meant "guys" in the generic sense.  Sorry, Tisha)
> Barry - N4BUQ
>
> ______________________________________________________________
> R-390 mailing list
> Home: http://mailman.qth.net/mailman/listinfo/r-390
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:R-390 at mailman.qth.net
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html 



More information about the R-390 mailing list