I use 2% silver solder routinely - I can't tell any difference. I'm told
that it sticks better to some surfaces, but the effect, if any, is subtle.
I did try the 4% silver solder but I didn't like it a bit - it doesn't
form a mirror surface - it hardens into a matte finish, so it is quite
hard to tell a cold solder joint from a proper one just by looking at it.
-A
On 2/27/2012 2:11 PM, Barry wrote:
> . . .
>
> Anyone try silver solder? I know it's used a lot in Tek scopes, etc., and haven't seen it much in old radios but was wondering.
>
> . . .
>
--