Back in the old days I used sodium hydroxide (lye) to "de-shine"
aluminum panels.   I seem to remember using a pretty strong
concentration in a glass Pyrex cake pan and a very thorough degreasing
was needed beforehand.   I'm fuzzy on this so I would try it out on a
piece of scrap panel first.

73 de Richard, W5SRB