[Elecraft] Crystals and ARC5s
N2EY at aol.com
N2EY at aol.com
Sat Jun 16 21:35:08 EDT 2007
In a message dated 6/16/07 5:05:09 PM Eastern Daylight Time, AJSOENKE at aol.com
writes:
> Then we'd disassemble the xtals and
> soak em in acid for a few minutes to tweak them up 3 or 5 KC.
What sort of acid?
The only acid I know that will etch acid is hydroflouric acid, (HF) which is
incredibly dangerous stuff.
There's a solution of ammonium biflouride that can do etching, which is not
nearly so nasty as HF - is that what you used?
73 de Jim, N2EY
**************************************
See what's free at
http://www.aol.com.
More information about the Elecraft
mailing list