[Elecraft] OT solder pot
thom2 at att.net
thom2 at att.net
Mon Feb 13 16:07:59 EST 2006
-------------- Original message ----------------------
From: Jim Wiley <jwiley at alaska.net>
>
> >
>
> I scrape the dross (oxidized solder and flux residue) from the surface
> of the solder bath as needed. I manufactured the scrapers by cutting
> strips of 0.010" stainless steel shim stock from a roll. Each scraper
> is about 1/2" wide and 6" long. The length allows you to scrape the
> dross before the heat transfers to your fingers. The solder won't stick
> to the stainless, so just scrape the dross off the tool with your
> fingernail or a utility knife when it has cooled.
>
>
Alternately, I've found that a nickel (a five cent coin, which is apparently not made of nickel) is also an adequate method of cleaning up the surface of the solder pot -- hold the nickel with a tweezer or pliers. The solder doesn't stick to the nickel either.
Tom WB2QDG
K2 1103