How to apply
The process goes as follows (50 years of perfecting) surface stripped to bare metal (important) prepped/cleaned with lacquer thinner, apply two thin coats 20 min apart , wait 10 min then apply a 250w heat lamp to achieve the wrinkle depth. The more heat the the deeper the wrinkle. Did a Collins 75A3 cabinet last year, applied a overcoat of St. James grey . Fabulous results . Heating the can in hot water helps, increased can pressure better atomizing . Only use a heat lamp not a gun ,heat guns with forced air dry the paint too quickly and have little control .