I think 60/40 was what we curmudgeons & our ancient ancestors were using for generations. There's a sort of excitement over 63/37 because it has a sharper freeze point temperature - IOW, it hardens somewhat faster when heat is removed. $6 for ~2ft of solder sounds like highway robbery.

Wayne
WB4OGM

On Sunday, May 5, 2024 at 11:51:36 AM MDT, [email protected] <[email protected]> wrote:


The last of my Radio Shack QQ-S-571 solder is about gone and I am wondering about replacement.  I only just noticed that the two most recent rolls of RS solder is 60/40 rather than 63/37.  I bought a little 63/37 on ebay, 25 inches for about $6, before I realized I was already using 60/40.  Which should we use?

I also found that desoldering WW2 vintage solder joints on the BC-348 using a 30 watt iron was not a good idea.  I bought a higher powqered iron, although I have a RS variable digital temp iron, I needed two for opposite sides of the workbench.

Wayne
WB5WSV 
______________________________________________________________
ARC5 mailing list
Home: http://mailman.qth.net/mailman/listinfo/arc5
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:[email protected]

This list hosted by: http://www.qsl.net
Please help support this email list: https://www.qsl.net/donate.html